PROCEDEU DE DENITRURARE A OŢELULUI TOPIT ÎN CURSUL ELABORĂRII SALE

Prețul nu e vizibil în cazul acestui pachet

Interes:

Atribuire

Informații publicare:

Nr.: RO121135

Data: 29.12.2006

Inventator(i):

MAILHAN JEAN-CHRISTOPHE [FR]

PERNET DANIEL [FR]

Aplicant(i):
USINOR [FR]
Clasificare:
Clasificare internationala (IPC):
C12C7/04; C21C5/52; C21C7/00; C21C7/04; C21C7/072; C22B9/05; C22B9/10; C22B9/00

Clasificare comuna (CPC):
C21C7/0025 (EP, KR, US); C21C7/0037 (EP, KR, US); C21C7/072 (EP, KR, US); F27D3/0026 (KR); F27D3/18 (KR)
Informații aplicație:
Nr.: RO19200100695
Data: 17.12.1999
Număr/numere prioritar(e):
FR19980016082 18.12.1998 ; WO1999FR03176 17.12.1999
Brevete asociate:
ATE246734; AU1664800; AU756853; BG105612; BR9916269; CA2356370; CN1329675; CZ20012225; DE69910256; EA003345; EA200100563; EP1141422; ES2205916; FR2787468; HU0104705; JP2002533566; KR20010101205; PL348064; SI20533; SK7932001; TR200101606; US6565622; WO0037688; YU42501; ZA200104661
Descriere:

Invenţia se referă la un procedeu de denitrurare a oţelului topit în timpul elaborării, destinat în special obţinerii oţelurilor cu conţinutredus de carbon. Procedeul conform invenţiei constă în injectarea în baia de metal topit de tratat, o dată, dar separat, în aceeaşi zonă a băii, a oxigenului şi carbonului sub o formă insuflabilă (de preferinţă, carbon pulverulent), generând local, în baie, bule de CO, pornind de laaceste două elemente, care merg să se încarce cu azot de denitrurare. O reglare stoechiometricăa aportului de carbon şi oxigen permite o denitrurare a carbonului constant din baie. Procedeul seaplică preferenţial la elaborarea sortimentelorde oţel cu un conţinut foarte scăzut de carbon, în special în cuptoare electrice.