PROCEDEU DE OBTINERE A POLIETERILOR GREFATI PENTRU SPUME POLIURETANICE FLEXIBILE

Price not visible for this package

Interest:

Assignment

Publication info:

No.: RO118302

Date: 30.04.2003

Inventor(s):

IONESCU MIHAI [RO]

ROIBU CONSTANTIN [RO]

PREOTEASA VERONICA [RO]

MIHALACHE IOANA [RO]

MIHAI STANCA [RO]

ZUGRAVU VIORICA [RO]

BEJENARIU IONEL [RO]

PUSCASU IULIANA [RO]

Applicant(s):
SC OLTCHIM SA [RO]
Classification:
International patent classification (IPC):
C08G18/50; C08G65/48

Cooperative patent classification (CPC):
Application info:
No.: RO20000000248
Date: 03.03.2000
Priority number(s):
RO20000000248 03.03.2000
Description:

Inventia se refera la un procedeu de obtinere a polieterilor grefati pentru spume poliuretanice flexibile, prin polimerizarea radicalica grefata a unor monomeri vinilici, intr-un mediu lichid constituit din polieteri polioli, homopolimeri ai propilenoxidului sau copolimeri propilenoxid-etilenoxid, cu rol de suport de grefare, si consta in aceea ca se adauga, la un prim amestec constituit din polieter, aproximativ 50...70% din polieterul necesar, stabilizatori de dispersie si poliol aminic, ca agent de transfer de lant, in concentratii de 2...10% fata de polieterul finit, aflat sub perna inerta de azot de 0,1...0,5 bari, la o temperatura de 80...130 degree C, un al doilea amestec, aflat la temperatura joasa de 5...30 degree C, constituit din polieter, in cantitate de 30...50% din polieterul necesar, stabilizatori de dispersie si poliol aminic, ca agent de transfer, monomeri vinilici, care reprezinta 10...50% din polieterul grefat, finit, preferabil stiren 50...100% si/sau acrilonitril 0...100%si initiator radicalic in concentratie de 2...8% fata de suma monomerilor vinilici, timp de 2...3 h, urmata de perfectarea reactiei timp de 1...1,5 h, la temperatura de 115...125 degree C, si degazarea masei de reactie la vid de 2...200 mmHg, cu barbotarea continua de azot pentru indepartarea monomerilor ramasi nereactionati.