ELECTROLIT DE ARGINTARE DURĂ A CONTACTELOR ELECTRICE

Price not visible for this package

Interest:

Assignment

Publication info:

No.: RO121140

Date: 29.12.2006

Inventor(s):

SACHIAN ARPIAR [RO]

MIHALCEA ARISTI A [RO]

Applicant(s):
INST DE CERCETARE I PROIECTARE [RO]
Classification:
International patent classification (IPC):
C25D3/00; C25D3/02; C25D3/46; C25D3/56; C25D3/64

Cooperative patent classification (CPC):
Application info:
No.: RO20020000892
Date: 21.06.2002
Priority number(s):
RO20020000892 21.06.2002
Description:

Invenţia se referă la un electrolit de argintare dură a contactelor elelctrice, care conţine 30...40 g/l argint metalic, 120...135 g/l KCN, 100 g/l K2CO3, 5...10 ml/l agent de durificare şi 0...0,60 ml/l produs de potenţare a acţiunii agentului de durificare. Numitul agent de durificare conţine 187 g trietanolamină, 7,5 g trioxid de stibiu, 21 g hidroxid de potasiu şi 30 g sare Seignette, amestecate şi complet dizolvate într-un volumde 250 ml soluţie apoasă, iar produsul de potenţare a acţiunii agentului de durificare conţine28% (vol.) compus având formula: Cl-CH2-CH2-Cl şi 72% (vol.) compus având formula HO-CH2-CH2-NH-CH2-CH2-NH2.